Txoj hauv kev tseem ceeb tshaj plaws los daws qhov tsis xws luag hauv kev ua cov castings yog "thermal balance". Txoj kev yog:
(1) Ceev ceev solidification yog nqa tawm nyob rau hauv cov tuab tuab thiab kub qhov chaw tsim los ntawm lub tshuab cuab tam casting qauv, artificially ua rau ib tug yooj yim tshuav nyiaj li cas ntawm qhov kub thiab txias teb txhua qhov chaw ntawm lub tshuab cuab yeej casting. Cov hlau txias sab hauv thiab sab nraud yog siv, thiab zircon xuab zeb, chromite xuab zeb los yog cov txheej tshwj xeeb nrog cov cua kub loj hauv zos.
(2) Tsim nyog txheej txheem tsim. Lub sab hauv khiav yog nyob rau ntawm phab ntsa ntawm lub tshuab cuab yeej casting, thiab feem ntau muaj ntau thiab tawg. Cov hlau molten uas nkag mus rau phab ntsa tuab thaum ntxov tshaj plaws yog solidified ua ntej, thiab cov phab ntsa nyias yog solidified tom qab, yog li ntawd uniform solidification yog yeej nyob txhua qhov chaw. Rau cov cuab yeej siv tshuab castings nrog cov phab ntsa tuab, siv ntau lub rooj vag thiab qhov cua. Muaj ntau cov sprues sab hauv, uas yog dispersed thiab sib npaug sib npaug kom sib npaug ntawm tag nrho cov cua sov. Cov cua qhov hluav taws xob yog nyias thiab ntau heev, uas txhais tau hais tias cov pa tawm yog du thiab plays lub luag haujlwm hauv cov cua kub dissipation.
(3) Hloov txoj haujlwm ntawm lub rooj vag
(4) Xaiv cov ntaub ntawv ua qauv nrog cov khoom siv hluav taws xob loj, uas yog qhov tseem ceeb heev rau kev tsim cov khoom siv los tiv thaiv cov khoom siv ua npuas ncauj ploj! Chromite xuab zeb hloov quartz xuab zeb thiab lwm hom xuab zeb nrog cov cua sov me me, uas yuav ua tiav cov txiaj ntsig zoo, thiab micro-shock tom qab nchuav yuav zoo dua!
(5) Tsis tshua muaj kub thiab kub kub ceev, qhib pouring system. Sau cov pwm nrog molten hlau sai, smoothly thiab tusyees. Qhov no nyob ntawm qhov xwm txheej.
(6) Cov cuab yeej siv lub tshuab hlau pwm muaj lub zog siab, qhov tawv tawv ntau dua lossis sib npaug ntawm 90, thiab cov xuab zeb lub thawv rigidity, uas muaj txiaj ntsig zoo rau kev tshem tawm cov porosity shrinkage.
(7) Thaum xav tau riser, txav lub riser kub ua ntej thiab tawm hauv qhov kub. Yog tias lub riser muab tso rau ntawm qhov kub, qhov loj ntawm riser yuav loj, uas ua rau "kub cua sov". Yog tias nws tsis ua tiav zoo, tsis yog tsuas yog yuav shrinkage thiab porosity yuav nyuaj rau tshem tawm, tab sis cov concentrated shrinkage kab noj hniav kuj yuav tshwm sim, uas yuav txo cov txheej txheem yield.
(8) Ob qho tib si tilted tso ntawm pwm thiab alloying yuav tau txais txiaj ntsig. Tshem tawm shrinkage thiab porosity defects nyob rau hauv lub tshuab cuab tam castings yog ib tug complex to taub thiab siv cov txheej txheem. "Thermal tshuav nyiaj li cas" yuav tsum tau siv raws li lub hauv paus ntsiab lus ntawm scientific soj ntsuam cov castings, tsim ib tug tsim nyog txoj kev npaj, xaiv cov khoom tsim nyog molding, cuab yeej, thiab ua hauj lwm kom raug thiab standardize. Tom qab ntawd cov shrinkage thiab porosity tsis xws luag ntawm txhua lub tshuab cuab yeej castings tuaj yeem daws tau.
Vim muaj kev cuam tshuam ntawm ntau yam, qhov tsis xws luag xws li pores, pinholes, slag inclusions, tawg, thiab pits feem ntau tshwm sim. Cov khoom siv kho mob feem ntau yog argon arc vuam tshuab, tsis siv lub vuam tshuab, txias vuam tshuab, thiab lwm yam. Casting defects uas tsis tas yuav tsum tau zoo thiab zoo li yuav kho nrog high-kub, ceev vuam tshuab xws li argon arc vuam tshuab. Txawm li cas los xij, hauv kev kho qhov tsis xws luag hauv precision castings, vim muaj zog ntawm argon vuam cua sov, kev kho yuav ua rau deformation ntawm casting, txo hardness, hlwv, hauv zos annealing, tawg, pinholes, hnav, khawb, undercuts, los yog tsis txaus. kev sib txuas ntawm lub zog thiab qhov tsis xws luag. Secondary defects xws li kev nyuaj siab puas. Lub tshuab vuam txias tsuas yog kov yeej cov teeb meem saum toj no. Nws cov txiaj ntsig tseem ceeb yog qhov chaw kub ntxhov me me, qhov casting tsis tas yuav tsum tau preheated, thiab txias vuam yog kho nyob rau hauv chav tsev kub, yog li tsis muaj deformation, undercut thiab residual stress, tsis muaj annealing hauv zos, thiab tsis muaj kev hloov nyob rau hauv lub. hlau ntawm casting. Lub koom haum xwm txheej. Yog li ntawd, lub tshuab txias vuam yog tsim los kho qhov tsis xws luag ntawm precision castings. Kev kho qhov txias ntawm vuam yog Φ1.5-Φ1.2mm, txheej txheem ntawm kev rov ua dua thiab sib sau ua ke ntawm cov ntsiab lus kho vuam. Nyob rau hauv tus txheej txheem ntawm kev kho qhov loj-qhov tsis xws luag, kho efficiency yog tib yam txwv tsis pub nws daim ntawv thov dav. Rau qhov tsis xws luag loj, kev sib xyaw ua ke ntawm cov khoom siv vuam tsoos kho tshuab thiab cov tshuab kho qhov tsis xws luag raug pom zoo. Tab sis qee zaum peb tsis muaj ntau yam tsis xws luag, yog li peb tsis tas yuav nqis peev nyiaj ntau. Peb tuaj yeem kho lawv nrog qee tus neeg ua haujlwm kho, uas yooj yim thiab yooj yim. Piv txwv li, rau cov khoom siv hlau, peb tuaj yeem siv (Jinsucheng) JS902 los kho lawv. Yog tias nws tsis siv, koj tuaj yeem muab tso rau tom qab siv. Qhov no tuaj yeem txuag nqi rau peb cov tuam txhab tsim khoom, tso cai rau peb cov tuam txhab tsim khoom lag luam los nqis peev nyiaj ntau hauv kev txhim kho cov khoom zoo ntawm lawv tus kheej, thiab tso cai rau cov neeg siv los tsim kev nplua nuj.